Nozzle Temperature: 190˚C – 230˚C
Printing Speed: 40mm/s – 60mm/s
Bed Temperature: 25˚C – 60˚C
Bed Surface: Glass with glue, Blue Tape, BuilTak®
Cooling Fan: ON
Mechanical Properties
Young’s Modulus: 2636 ± 330 Mpa
Tensile Strength: 46.6 ± 0.9 Mpa
Bending Strength: 85.1 ± 2.9 Mpa
Charpy Impact Strength: 2.7 ± 0.2 kJ/m2
Thermal Properties
Glass Transition Temperature: 61˚C
Vicat Softening Temperature: 63˚C
Melting Temperature: 150˚C